When comparing UV DTF inks, ask for ASTM D3359 cross-cut results, not just “strong adhesion” claims. The 0B-to-5B scale records how much coating lifts after a grid is cut and tape is applied. At 5B, no squares detach; at 4B, less than about 5% is removed. Ratings descend as more material comes away, with 0B indicating extensive removal. That matters.
Treat the number as a comparison, not a universal promise. Test the same film, receiving surface, cleaning method, curing conditions, and tape whenever possible. A high rating on glass may not predict performance on a textured plastic panel. D3359 was developed for coating adhesion, so check whether the test setup suits the complete UV DTF transfer. The ink, adhesive, film, and surface all affect the result.
Ask for the test method, substrate, and sample preparation behind each rating. If the details are missing, request cured samples and repeat the cross-cut test under consistent conditions. Inspect the grid under good light; note peeling at the cuts, not only large flakes. One excellent coupon is still only a clue, not proof. Real handling, moisture, and repeated contact can expose weaknesses that a single test misses.